BS X2CrNiN18-10
2015-03-26 09:28:16 Origin: Remark:0 Click:
BSEN Austenitic stainless steel material specification X2CrNiN18-10 datasheet,BS EN X2CrNiN18-10 Chemical, Ring forging,EN X2CrNiN18-10 Bar, Wire rod, Sheet - steelmaking, ESR, Blooming, Forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION / DATASHEET - BS X2CrNiN18-10 /1.4311
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C(%): ≤0.030
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.030
Cr(%): 17.0~19.5
Ni(%): 8.50~11.5
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.030
Cr(%): 17.0~19.5
Ni(%): 8.50~11.5
Mo(%): -
Other(%): N0.12~0.22
MECHANICAL PROPERTIES ( BAR/WIRE ROD ) AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 230
Yield strength σ0.2≥/MPa: 270
Tensile strength σb/MPa: 550~760
Elongation δ(longitudinal )≥(%): 40
Yield strength σ0.2≥/MPa: 270
Tensile strength σb/MPa: 550~760
Elongation δ(longitudinal )≥(%): 40
Elongation δ(transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: 100
Impact absorbing energy Akv≥/J|transversal: —
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Impact absorbing energy Akv≥/J|transversal: —
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Thickness Diameter (d)/≤mm: 160<d≤250