BS EN 1.4305
2015-03-28 09:06:01 Origin: Remark:0 Click:
BSEN Austenitic stainless steel material specification EN 1.4305 datasheet,EN 1.4305 Chemical, Ring forging,EN 1.4305 Bar, Wire rod,EN 1.4305 Sheet - steelmaking, ESR, Blooming, Forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION / DATASHEET - BS X8CrNiS18-9 /1.4305
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C(%): ≤0.10
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.015~0.35
Cr(%): 17.0~19.0
Ni(%): 8.00~10.0
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.015~0.35
Cr(%): 17.0~19.0
Ni(%): 8.00~10.0
Mo(%): -
Other(%): N≤0.11,Cu≤1.00
MECHANICAL PROPERTIES ( BAR/WIRE ROD ) AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 230
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~750
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~750
Elongation δ(longitudinal )≥(%): 35
Elongation δ(transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: -
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: No
Intergranular corrosion resistance tendency | condition of welding: No
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: No
Intergranular corrosion resistance tendency | condition of welding: No
Thickness Diameter (d)/≤mm: 160<d≤250