BS X4CrNi18-12
2015-03-28 09:40:53 Origin: Remark:0 Click:
BSEN Austenitic stainless steel material specification X4CrNi18-12 datasheet,X4CrNi18-12 Chemical, Ring forging, EN X4CrNi18-12 Bar, Wire rod, BSEN X4CrNi18-12 Sheet - steelmaking, ESR, Blooming, Forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION / DATASHEET - BS X4CrNi18-12 /1.4303
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C(%): ≤0.060
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.030
Cr(%): 17.0~19.0
Ni(%): 11.0~13.0
Mo(%): —
Other(%): N≤0.11
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.030
Cr(%): 17.0~19.0
Ni(%): 11.0~13.0
Mo(%): —
Other(%): N≤0.11
MECHANICAL PROPERTIES ( BAR/WIRE ROD ) AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 215
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~700
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~700
Elongation δ(longitudinal )≥(%): 45
Elongation δ(transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: 100
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: No
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: No
Thickness Diameter (d)/≤mm: 160<d≤250