EN 1.4303
2015-03-29 14:02:35 Origin: Remark:0 Click:
BSEN Austenitic stainless steel material specification EN 1.4303 data sheet, EN 1.4303 Chemical, Ring forging,EN 1.4303 Bar, Wire rod, BSEN 1.4303 Sheet - steelmaking, ESR, Blooming, Forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION DATASHEET - BS X4CrNi18-12 & 1.4303
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C (%): ≤ 0.060
Si (%): ≤ 1.00
Mn (%): ≤ 2.00
P (%)≤: 0.045
S (%)≤: 0.030
Cr (%): 17.0 ~ 19.0
Ni (%): 11.0 ~ 13.0
Mo (%): —
N (%): ≤ 0.11
Si (%): ≤ 1.00
Mn (%): ≤ 2.00
P (%)≤: 0.045
S (%)≤: 0.030
Cr (%): 17.0 ~ 19.0
Ni (%): 11.0 ~ 13.0
Mo (%): —
N (%): ≤ 0.11
MECHANICAL PROPERTIES ( BAR/WIRE ROD ) AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 215
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~700
Yield strength σ0.2≥/MPa: 190
Tensile strength σb/MPa: 500~700
Elongation δ(longitudinal )≥(%): 45
Elongation δ(transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: 100
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: No
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: No
Thickness Diameter (d)/≤mm: 160<d≤250