EN 1.4406
2015-03-29 14:17:35 Origin: Remark:0 Click:
Specification 1.4406 datasheet, 1.4406 Chemical, Ring forging 1.4406 Bar, Wire rod, steelmaking, ESR, Blooming, Hot forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION DATASHEET - 1.4406
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C (%): ≤ 0.030
Si (%): ≤ 1.00
Mn (%): ≤ 2.00
P (%)≤: 0.045
S (%)≤: 0.030
Cr (%): 16.5 ~ 18.5
Ni (%): 10.0 ~ 12.0
Mo (%): 2.00 ~ 2.50
Si (%): ≤ 1.00
Mn (%): ≤ 2.00
P (%)≤: 0.045
S (%)≤: 0.030
Cr (%): 16.5 ~ 18.5
Ni (%): 10.0 ~ 12.0
Mo (%): 2.00 ~ 2.50
N (%): 0.12~0.22
MECHANICAL PROPERTIES AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 250
Yield strength σ0.2≥/MPa: 280
Tensile strength σb/MPa: 580~800
Yield strength σ0.2≥/MPa: 280
Tensile strength σb/MPa: 580~800
Elongation δ (longitudinal )≥(%): 40
Elongation δ (transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: 100
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Thickness Diameter (d)/≤mm: 160<d≤250