BS X2CrNiMoN17-13-3
2015-03-30 09:34:35 Origin: Remark:0 Click:
BSEN Austenitic stainless steel material specification X2CrNiMoN17-13-3 datasheet,X2CrNiMoN17-13-3 Chemical, Ring forging,BSEN X2CrNiMoN17-13-3 Bar,Wire rod, Sheet -steelmaking,ESR, Blooming, Forging, Rolling, Heat treatment, Straightened, Ultrasonic test, Cold working, Machined. We also possess advanced precision machining equipments for further processing.
Technical Standards - BS EN 10088-3 (2005) or by agreement.
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
TECHNICAL SPECIFICATION / DATASHEET - BS X2CrNiMoN17-13-3 /1.4429
MATERIAL CATEGORY: Stainless steel round bar, wire rod, and semi-finished products
STEEL TYPE: Austenitic series
MATERIAL SPECIFICATIONS: BS EN 10083-3 (2005)
CHEMICAL COMPOSITION (WEIGHT %)
C(%): ≤0.030
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.015
Cr(%): 16.5~18.5
Ni(%): 11.0~14.0
Mo(%): 2.50~3.00
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.045
S(%)≤: 0.015
Cr(%): 16.5~18.5
Ni(%): 11.0~14.0
Mo(%): 2.50~3.00
Other(%): N0.12~0.22
MECHANICAL PROPERTIES ( BAR/WIRE ROD ) AND INTERGRANULAR CORROSION RESISTANT TENDENCY VIA SOLUTION TREATMENT
Thickness Diameter (d)/≤mm: 160
Hardness HBS: 250
Yield strength σ0.2≥/MPa: 280
Tensile strength σb/MPa: 580~800
Yield strength σ0.2≥/MPa: 280
Tensile strength σb/MPa: 580~800
Elongation δ(longitudinal )≥(%): 40
Elongation δ(transversal )≥(%): -
Impact absorbing energy Akv≥/J|longitudinal: 100
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Impact absorbing energy Akv≥/J|transversal: -
Intergranular corrosion resistance tendency | condition of delivery: Yes
Intergranular corrosion resistance tendency | condition of welding: Yes
Thickness Diameter (d)/≤mm: 160<d≤250