NF EN X2CrNiZr17
2017-02-28 09:15:15 Origin: Remark:0 Click:
Material technical specifications of NF EN 10088-2 2005 type EN X2CrNiZr17 stainless steel plate and strip EN X2CrNiZr17 datasheet, EN X2CrNiZr17 Chemical compositions, mechanical properties from Steelmaking, ESR melting, Hot blooming,UT, X2CrNiZr17 Hot forging, Hot rolling, X2CrNiZr17 Heat treatment, Straightening, 100% Ultrasonic test, Cold working or Machined. Technical specifications - NF EN 10088-2 2005. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
TECHNICAL SPECIFICATION & DATASHEET - NF EN X2CrNiZr17
TYPE OF STEEL: Special Grade
OFFICIAL TEST CERTIFICATE: issued by TUV - SGS - BV
MATERIAL CATEGORY: Stainless Steel Plate and Strip
Technical standards: NF EN 10088-2 2005
CHEMICAL COMPOSITION (WEIGHT %)
C (%): ≤ 0.030
Si (%): ≤ 1.00
Mn (%): ≤ 1.00
P (%)≤: 0.040
S (%)≤: 0.015
Cr (%): 16.0 ~ 17.5
Mo (%): -
Ni (%): -
Nb (%): 0.35 ~ 0.55
Zr (%): 7 X ( C+N ) + 0.15
MECHANICAL PROPERTIES UNDER ROOM TEMPERATURE
Condition: cold rolled steel strip
Tensile strength,σb/≥ MPa: 480 ~ 550
Yield strength, σ0.2/≥ MPa: 250
Elongation, δ ≥(%): 23.0
PRODUCT DESCRIPTION
The alloy is usually produced by AOD / VOD /VIM followed by electroslag refining (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied black/bright in the annealed condition.
Final heat treatment - solution treatment
HEAT TREATMENT PRACTICE
Heat treatment is only suitable for specific grades of stainless steel. When heat treating a stainless the hardening temperatures, including rate of heating, cooling and soaking times will vary due to several factors such as the shape and size of each component. Other considerations during the heat treatment process include the type of furnace, quenching medium and work piece transfer facilities. Please consult with the heat treatment provider for whole guidance on heat treatment of stainless steel grades. We are delighted to help to work with you the special heat treatment based on your special requirements.
PRODUCT PROFILE
Heavy/middle plate via hot rolled: T3 - 200mm X W1000- 2500mm X L1000-12000mm
Sheet steel via cold rolled: T0.5 - 3mm X W600- 1000mm X L1000 - 2000mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 600mm X L (or in coil form)
MECHANICAL PROPERTIES UNDER ROOM TEMPERATURE
Condition: cold rolled steel strip
Tensile strength,σb/≥ MPa: 480 ~ 550
Yield strength, σ0.2/≥ MPa: 250
Elongation, δ ≥(%): 23.0
PRODUCT DESCRIPTION
The alloy is usually produced by AOD / VOD /VIM followed by electroslag refining (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied black/bright in the annealed condition.
Final heat treatment - solution treatment
HEAT TREATMENT PRACTICE
Heat treatment is only suitable for specific grades of stainless steel. When heat treating a stainless the hardening temperatures, including rate of heating, cooling and soaking times will vary due to several factors such as the shape and size of each component. Other considerations during the heat treatment process include the type of furnace, quenching medium and work piece transfer facilities. Please consult with the heat treatment provider for whole guidance on heat treatment of stainless steel grades. We are delighted to help to work with you the special heat treatment based on your special requirements.
PRODUCT PROFILE
Heavy/middle plate via hot rolled: T3 - 200mm X W1000- 2500mm X L1000-12000mm
Sheet steel via cold rolled: T0.5 - 3mm X W600- 1000mm X L1000 - 2000mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 600mm X L (or in coil form)
TECHNICAL SALES ASSISTANCE
If you meet further on any technical enquiry. pleased to EMAIL our resident team of qualified production engineers.
Email: lh.steel@hotmail.com
Hot search:NF EN X2CrNiZr17
Previous page:SK75M/SK6M
Last page:Hastelloy C-276 / N10276
Total list
Monthly rank
- 24X35CrMo17
- 23Z15CN17-03
- 23ASTM A565 Gr.616HT
- 21X10CrNiW17-13-3
- 19ASTM A638 Gr.660
- 18AISI 306
- 15SAE 51420
- 14P550
- 14SAE 51416
- 14X12CrMoWVNbN10-1-1