X3CrNiN17-8 Stockist, X3CrNiN17-8 Equivalent Steel

X3CrNiN17-8
2017-07-26 10:23:04   Origin:   Remark:0 Click:

NF FD A35-570 -1996 Stainless steel X3CrNiN17-8 Round bar, Flat bar, Plate, X3CrNiN17-8 ESR melting, Hot blooming, UT, Hot forging, Hot rolling, Heat treatment.
TECHNICAL DATASHEET - NF X3CrNiN17-8

OFFICIAL TEST CERTIFICATE: issued by TUV - SGS -  BV
MATERIAL CATEGORY: Stainless 
Steel Flat or plate 
Technical standards: NF FD A35-570 - 96 
CHEMICAL COMPOSITION (mass weight - %)
Carbon, C (%):  ≤ 0.050
Silicon, Si (%):  ≤ 1.00
Manganese, Mn (%):  ≤ 2.00
Phosphorus, P (%)≤:  0.045
Sulfur, S (%)≤:  0.015
Chromium, Cr (%):  16.0 ~ 18.0
Molybdenum, Mo (%):  -
Nickel, Ni (%):  7.00 ~ 8.00
Nitrogen, N (%):  0.04 ~ 0.08
MECHANICAL PROPERTIES UNDER ROOM TEMP.
Tensile strength,σb/≥ MPa: 515
Yield strength, σ0.2/≥ MPa: 205
Elongation, δ ≥(%): 40.0
Reduction of area, (%): 55.0
Annealed hardness, HB ≤: -
PRODUCT DESCRIPTION
The
alloy is usually produced by AOD / EF / EAF followed by electroslag refining (ESR) / VAR if necessary for special purpose. Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied black/bright in the annealed condition.
Final heat treatment - Quenched and tempered thermal treatment
PRODUCT PROFILE
Round bar & Disc (diameter): 5.50 to 600mm
Square bar / Flat bar: T3.0 to 500mm X W3.0 ~ 1200mm
Length: Fixed length or random length or based on the customer's special requirement.
Heavy/middle plate via hot rolled: T3.0 - 200mm X W1000- 2500mm X L1000-12000mm.
TECHNICAL SALES ASSISTANCE
If you meet further on any technical enquiry, you can do as follows EMAIL our qualified production engineers,  Email:
sales@ccsteels.com 

Hot search:X3CrNiN17-8