ASTM A276 Specifications S40940 Round bar, Flat bar, Plate S40940 (EF / VIM ), ESR & VAR technique, Blooming, Hot forging, Hot rolling, Heat treatment
 
TECHNICAL DATA SHEET - S40940
 
TECHNICAL SPECIFICATIONS - ASTM A276 & A182 & A240
OFFICIAL TEST CERTIFICATE - issued by TUV - SGS -  BV
MATERIAL CATEGORY - Ferritic stainless
steel
 
TYPICAL CHEMICAL COMPOSITION (mass weight - %)
Carbon, C (%): ≤ 0.06
Silicon, Si (%): ≤ 1.00
Manganese, Mn (%): ≤ 1.00
Phosphorus, P (%) ≤: 0.045
Sulfur, S (%) ≤: 0.040
Chromium, Cr (%): 10.5 ~ 11.7
Nickel, Ni (%): ≤ 0.50
Molybdenum, Mo (%): -
Niobium, Nb (%): 10×C ~ 0.75

MECHANICAL PROPERTIES UNDER ROOM TEMP.
Form: Bar, plate, strip and forgings
Tensile strength, Rm / MPa:  317
Yield strength, Rp0.2 / MPa: 225
Elongation, A5 (%): 20.0
Rudction of area, Z (%): -
Hardness (HBW): -
Hardness | HRB:  -
Cold bending property: N

 
METHOD OF MELTING
The
alloy is usually produced by AOD / EAF / VIM, followed by electroslag refining (ESR or VAR ) if necessary for special purpose.
 
AVAILABLE FORMS & DIMENSIONS
Round bar / Disc (diameter): 5.5 ~ 850mm
Wire rod (Diameter): 0.15 ~ 15mm
Flat bar (Thickness X Width): 10 ~ 400 X 15 ~ 650mm
Length: random length, fixed length or based on the customer's special requirement.
Form: wire or straightened bar

 
TECHNICAL SALES ASSISTANCE
If you meet further on any technical inquiry, pleased to EMAIL our resident team of qualified production engineers, Email us:
sales@ccsteels.com.

Hot search:S40940

Previous page:409Cb
Last page:UNS S40945

Share to: