DATA SHEET - Alloy Steel - ASTM 420F & UNS S42020
PRODUCT DESCRIPTION
The alloy is usually produced by AOD / VOD /VIM followed by electroslag refining (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied black/bright in the annealed condition.
Final heat treatment - solution treatment / QT
MATERIAL SPECIFICATIONS
ASTM A959 (2004), A276, A312, A632, A176, A580
CHEMICAL COMPOSITION (WEIGHT %)
Si (%): ≤ 1.00
Mn (%): ≤ 1.25
P (%)≤: 0.060
S (%)≤: ≥ 0.15
Cr (%): 12.0 ~ 14.0
Ni (%): —
Mo (%): ≤ 0.60
MECHANICAL PROPERTIES ( FINAL HEAT TREATMENT OR Q/T)
σ0.2/MPa: 760
ф(%): -
Hardness | HRB: -
Chemical equipment
Mechanical parts used in the condition of corrosion resistance
Bolt and nut
Pressure vessel
TECHNICAL SALES ASSISTANCE
If you meet further on any technical enquiry. pleased to EMAIL our resident team of qualified production engineers. - Email: sales@ccsteels.com
Previous page:ASTM 420F
Last page:ASTM 420FSe
Total list
Monthly rank
- 24X35CrMo17
- 23Z15CN17-03
- 23ASTM A565 Gr.616HT
- 21X10CrNiW17-13-3
- 19ASTM A638 Gr.660
- 18AISI 306
- 15SAE 51420
- 14P550
- 14SAE 51416
- 14X12CrMoWVNbN10-1-1