53Cr21Mn9Ni4N Stockist, 53Cr21Mn9Ni4N Equivalent Steel

53Cr21Mn9Ni4N
2024-07-13 15:47:10   Origin:   Remark:0 Click:

GB/T 1221 Material Specification Heat Resistant & Austenitic Steel 53Cr21Mn9Ni4N Round bar, Flat bar, Plate, Forgings 53Cr21Mn9Ni4N Stock Available

MATERIAL DATASHEET - GB 53Cr21Mn9Ni4N

Official Test Report: issued by TUV - SGS -  BV
Special Melting Practice - BEF + AOD / + ESR
HS Code - 72223000 / 72224000
Stock Available - Round bar Diam. 10 ~  60mm

Material Specifications - GB/T 1221 -2007 Heat Resisting Steel
 
PRODUCT DESCRIPTION
The alloy is usually produced by EAF / AOD / BEF followed by electroslag refining (ESR) / VAR if necessary for special purpose. Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied black/bright in the annealed condition.
Final heat treatment - solution annealing (+ AT).

PROFILE & DIMENSIONS & PROCESSING SERVICE
Round bar & Disc (diameter): 5.5 ~ 600mm
Square bar / Flat bar: 6 ~ 650mm
Length: Fixed length or random length or based on the customer's special requirement.
Heavy / middle plate via hot rolled: T10 ~ 410 X W20 ~ 1000 X Lmm
Sheet steel via cold rolled: T0.5 - 6 X W60 ~ 1000 X Lmm
Steel strip via cold rolled: T0.1 - 3 X W5 - 1000 X L (or in coil form)
Forging piece: stepped shafts, other different shapes based on OEM.
 
We closely cooperate with the professional inspection partners to strictly control the quality and improve the quality manage system, and guarantee the goods delivery each time. It is proved that we are worth of trusting and will be the strategic partner of the supplying chains in the special steels field.
Export packing / Export documents.
Transport by Track, Sea, Courier (FedEx, UPS, DHL) and Air Cargo.
CNC saw cutting.
Marking by stamping or printing.
Third party inspection service.
 
MAIN CHEMICAL ELEMENTS ( ladle analysis - %)
Carbon, C (%): 0.48 ~ 0.58
Silicon, Si (%): ≤ 0.35
Manganese, Mn (%): 8.00 ~ 10.0
Phosphorus, P (%) ≤: 0.040
Sulfur, S (%) ≤: 0.020
Chromium, Cr (%): 20.0 ~ 22.0
Nickel, Ni (%): 3.25 ~ 4.50
Molybdenum, Mo (%): -
Nitrogen, N (%): 0.35 ~ 0.50

MECHANICAL PROPERTY AT ROOM TEMPERATURE
Forms: Round bar, flat bar, forgings and plate
Heat treatment practice: solution annealing 1100 ~ 1200 ℃, quick cooling.
                                       aged 730 ~ 780 ℃, air cooling.
Tensile strength, Rm ≥ MPa: 885
Yield strength, Rp0.2  MPa: 560
Elongation, A ≥ (%): 8.0
Reduction of area, Z ≥ (%):  -
Hardness via annealing /HBW:  302 Min.

TECHNICAL SALES ASSISTANCE & SERVICE
20+ years Focus On Special Steel Manufacturing and processing.
Stock over 60 grades with a competitive price, along with cutting service for specific requirement.
Customizing special material is welcome.