E35NCD16H Stockist, E35NCD16H Equivalent Steel

E35NCD16H
2019-12-23 09:01:53   Origin:   Remark:0 Click:

Stocklist E35NCD16H Specifications, Inventory E35NCD16H Chemical, Suppliers E35NCD16H Forge bar plate machined, ESR & VAR technique, Hot forging, Hot rolling, Heat treatment.
TECHNICAL SPECIFICATION - Grade E35NCD16H

TECHNICAL SPECIFICATION - DGA - AIR 9160/C  - 1973
OFFICIAL TEST CERTIFICATE - issued by TUV - SGS
MATERIAL CATEGORY - Low alloy
structural steel
CHEMICAL COMPOSITION (mass weight % )
Carbon, C (%):  0.30 ~ 0.40
Silicon, Si (%):  0.15 ~ 0.40
Manganese, Mn (%):  0.30 ~ 0.60
Phosphorus, P (%) ≤:  0.020
Sulfur, S (%) ≤:  0.020
Chromium, Cr (%):  1.60 ~ 2.00
Molybdenum, Mo (%):  0.25 ~ 0.60
Nickel, Ni (%):  3.50 ~ 4.50
MECHANICAL PROPERTIES UNDER ROOM TEMPERATURE
Tensile strength,σb/≥ MPa: 1230 ~ 1360
Yield strength, σ0.2/≥ MPa: 1030
Elongation, δ ≥(%): 10.0
Reduction of area, ф ≥ (%): 40.0
Impact, AK (J/cm2): -
Heat treated hardness | HB: 363 ~ 415
Quenching, 875,+/-10 Deg X 3h, tempering 560, +/-5 Deg, air cooling
FEATURE AND AVAILABLE FORMS
35NCD16 is a low alloy steel which combines high strength and hardenability with good dimensional stability, making it an excellent alloy for large section mechanical parts or tooling of complex shapes subject to high stressses.
Round bar (Diameter): 5.5 mm to 500mm
Square bar / Flat bar: 10mm to 500mm
Steel strip: T0.50 ~ 3mm X W10 ~ 400mm X Coil
Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
TECHNICAL SALES ASSISTANCE
If you meet further on any technical enquiry or help, pleased to EMAIL (
sales@ccsteels.com) our resident team of qualified production engineers.

Hot search:E35NCD16H

Previous page:AMS 6495
Last page:STS431

Share to: