BS 970-5 Specifications EN50 Round bar, Flat bar, Plate EN 50 Properties from Steelmaking, Hot forging, Hot rolling, Heat treatment
 
TECHNICAL DATA SHEET - EN50

MATERIAL CATEGORY - low alloy steel with high tensile
TECHNICAL SPECIFICATION - BS970 Part 5
MELTING: Consumable electrode remelted
OFFICIAL TEST REPORT - issued by TUV - SGS -  BV
CHEMICAL COMPOSITIONS (mass fraction - %)
Carbon, C (%): 0.40 ~ 0.50
Manganese, Mn (%): 0.50 ~ 0.70
Silicon, Si (%): 0.10 ~ 0.35
Phosphorus, P (%) ≤: 0.035
Sulfur, S (%) ≤: 0.025
Chromium, Cr (%): 1.00 ~ 1.50
Nickel, Ni (%): -
Molybdenum, Mo (%): -
MECHANICAL PROPERTY AND HARDNESS
Quenching temperature /℃:840, oil cooled
Tempering temperature /℃:520
Tensile strength, Rm ≥ MPa: 1030
Yield strength, Rp0.2 ≥ MPa: 835
Elongation, A5 ≥ (%): 9.0
Reduction of area, Z (%): 40.0 min.
Hardness in condition of annealing +A: HB229 max.
MELTING PROCESS & APPLICATION
This
alloy is generally smelt in Electric Arc Furnace  (EAF), EAF+LF+VD, BEF + Electroslag remelting (ESR). For a purpose of superior quality, it should be smelt via technology of vacuum refining or by agreement.
It is suitable for applications such as high tensile shafts, bolts and nuts, gears, pinions spindles and so on. 
AVAILABLE FORMS & DIMENSIONS
Round bar: 5.5mm to 400mm
Square bar / Flat bar: 10mm to 550mm
Length: Fixed length or random length or based on the customer's special requirement.
Other different shapes based on OEM.  
TECHNICAL SALES ASSISTANCE & SERVICE
If you meet further on any technical enquiry, pleased to EMAIL (sales@ccsteels.com) our resident team of qualified production engineers

Hot search:

Previous page:T51621
Last page:STR 600

Share to: