NCF825
2021-08-09 13:48:53   Origin:   Remark:0 Click:

Specifications NCF825 Datasheet, Inventory NCF825 Chemical, Suppliers NCF825 Stcoklist Property Technical specifications - KS D3531 - 2003. From Melting - ESR & VAR technique, Blooming, Hot forging, Hot rolling, Heat treatment, Straightening, 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
TECHNICAL DATASHEET - Grade NCF825

Technical Specifications - KS D3531 - 1992/2003
Official Test Certificate - issued by TUV - SGS -  BV
Material Category - Heat resistant stainless
steel & Superalloy
Chemical Composition ( Mass Weight % )
C (%):     ≤ 0.05
Si (%):     ≤ 0.50
Mn (%):   ≤ 1.00
P (%) ≤:  0.030
S (%) ≤:  0.015
Cr (%):    19.0 ~ 23.0
Ni (%):    38.0 ~ 46.0
Mo (%):   1.50 ~ 3.50
Tensile strength, σb/ ≥ MPa: 580
Yield strength, σ0.2/ ≥ MPa: 235
Elongation, δ (%) ≥: 30.0
Reduction of area, ф (%) ≥: -
Hardness under solution anneal ≤ (HBW): -
MELTING PROCESS
The
alloy is usually produced by AOD / EAF / VIM, followed by electroslag refining (ESR or VAR ) if necessary for special purpose.
AVAILABLE FORMS & DIMENSIONS
Round bar (Diameter): 5.5 ~ 400mm
Wire rod (Diameter): 0.15 ~ 13mm
Flat bar (Thickness X Width): 4 ~ 300 X 15 ~ 600mm
Length: random length, fixed length or based on the customer's special requirement.
Form: wire or straightened bar
TECHNICAL SALES ASSISTANCE
If you meet further on any technical inquiry or help, pleased to EMAIL our resident team of qualified production engineers, Email us:
sales@ccsteels.com.  

Hot search:NCF825

Previous page:EN 58H
Last page:NCF80A

Share to: