BA2 /1.2363
2016-01-19 12:53:21   Origin:   Remark:0 Click:

Technical specifications of BS standards Cold work alloy tool steel BA2 datasheet, BA2 /1.2363 Chemical compositions, BA2 /1.2363 Mechanical properties from Steelmaking, ESR melted, Blooming, Hot forging, Hot rolling, Heat treatment, Straightening, 100% Ultrasonic test, Cold working, Peeled or rough turned machining. Technical specification - BS 4659/1989. We also possess the advanced precision machining equipments for catering for your different special requirements.
 
 
Technical  Data Sheet: BA2 /1.2363

OFFICIAL TEST REPORT: issued by TUV - SGS BV
MATERIAL CATEGORY:  Cold work alloy tool steel
MATERIAL SPECIFICATIONS:  BS 4659 - 89
CHEMICAL COMPOSITION (WEIGHT - %)
C (%):     0.95~1.05
Si (%):     ≤0.40
Mn (%):   0.30~0.70

P (%)≤:   0.030
S (%)≤:   0.030
Cr (%):    4.75~5.25
Mo (%):   0.90~1.10
W (%):     -
V (%):      0.15~0.40
HEAT TREATMENT PRACTICE AND HARDNESS
Annealing temperature ℃:                       850~870
Hardness after annealing ≤HBW:               241

Preheating temperature  ℃ /:                   800
Quenching temperature ℃:                       950~980
Cooling medium:                                      air cooled
Tempering temperature ℃:                      150~350
Hardness value after tempered /≥ HV:        735

MELTING PROCESS 
This alloy is generally smelt in electric arc furnace  (EAF ) or IFF + VD, LF + Electroslag remelting (ESR).
For a purpose of higher quality, it should be smelt via technology of vacuum refining.
TYPICAL APPLICATIONS
Alloy tool steel is widely used to produce the cutting tool, cold/heat distortion mould and measuring implements,
and further to manufacture the piston, valve, valve seat of fuel pump of diesel engine.
Cutlery for medical equipments
Cutting tools
Mechanical parts 
Air hammer tools
Piercing tools
HEAT TREATTMENT PRACTICE
The preheating of measuring and cutting
tool steel is spheroidizing annealing, final heat treatment is quenching + low temperature tempering and hardness after heat treatment can reach 60~65HRC. When heat treat tool steel grades consideration should be given to hardening temperature, including ratio of heating, cooling and soaking times which will differ due to factors such as the shape and size of each chemical component. Other considerations during heat treatment include the type of furnace, quenching medium and work piece transfer facilities.
PRODUCT PROFILE
Round bar (Diameter):  0.50mm to 800mm
Square bar / Flat bar:   3mm to 800mm
Length: Fixed length or random length or based on the customer's special requirement.
Steel strip: T0.20 ~ 3mm X W10 ~ 2000mm X Coil
Heavy/middle plate via hot rolled: T4 - 200mm X W1000- 2500mm X L1000-12000mm
Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.  

TECHNICAL SALES ASSISTANCE & SERVICE
If you meet further on any technical enquiry. pleased to EMAIL our resident team of qualified production engineers.
- Email us:
lh.steel@hotmail.com
  

Hot search:BA2 /1.2363

Previous page:BA2 /SKD12
Last page:80MoCrV42-16 /B60

Share to: