Material Standard SIS EN ISO 4957 Tool steel SS 1770 Round bar, Flat bar, ESR melted, Hot forging, Hot rolling, Heat treatment, Cold working.
 
TECHNICAL DATA SHEET: SS 1770

MATERIAL CATEGORY: Carbon tool steel
MATERIAL SPECIFICATIONS: SIS EN ISO 4957 -2001
CHEMICAL COMPOSITIONS (mass fraction - %)
Carbon, C (%): 0.65 ~ 0.75
Silicon, Si (%): 0.15 ~ 0.40
Manganese, Mn (%): 0.60 ~ 0.80
Phosphorus, P (%) ≤: 0.030
Sulfur, S (%) ≤: 0.030
HOT WORKING, HEAT TREATMENT PRACTICE AND HARDNESS
Hot working temperature /℃: 1000 ~ 750
Annealing temperature /℃: 750
Annealed hardness, ≤ HB: 200
Quenching temperature /℃: 800 ~ 820
Cooling medium: water
Tempering temperature /℃: 140 ~ 200
Hardness under tempered condition ≥HRC: 62 ~ 56
MELTING PROCESS
This
alloy is generally smelt in Electric Arc Furnace  (EAF), EAF+LF+VD, LF + Electroslag remelting (ESR).
For a purpose of superior quality, it should be smelt via technology of vacuum refining or by agreement.

PROFILE AND DIMENSIONS
Round bar (Diameter): 5.50 to 550mm
Square bar / Flat bar: T3 to 500mm X W3 ~ 1200mm
Steel strip: THK0.15 ~ 2.50 X W8.0 ~ 185mm
Length: Fixed length or random length or based on the customer's special requirement.
Other different shapes based on OEM.
TECHNICAL SALES ASSISTANCE & SERVICE
If you meet further on any technical enquiry. pleased to EMAIL our resident team of qualified production engineers. Email: sales@ccsteels.com

Hot search:SS 1770

Previous page:STF8
Last page:DTD 5052

Share to: