37CrNi3A Stockist, 37CrNi3A Equivalent Steel
Home > Tool steel > Text

37CrNi3A
2024-11-29 10:39:37   Origin:   Remark:0 Click:

GJB 1951-94 Material Specification for Quality Structure Steel Bars for Aviation 37CrNi3A ESR ingot, Stock Available Round bar, Flat bar 37CrNi3A Forgings
 
MATERIAL DESIGNATION - GB 37CrNi3A

MATERIAL CATEGORY - Sp
ecification for Quality Structure Steel Bars for Aviation.
 
TYPICAL APPLICATIONS
Alloy structural 
steels are widely used in the filed of ship, vehicle, airplane, guided missile, weapons, railway, bridges, pressure vessel, machine tools, mechanical components with a bigger sectional size and so on. 
Mechanical parts - connecting rod, bolt and nuts.
Multidiameter shaft, Pressure vessel parts.
Power generation – turbine fasteners – boiler support rods.
Process plant – fasteners, Mechanical gears, gear shaft, main axis, valve rod.

PRODUCT DESCRIPTION
The 
alloy is usually produced by EAF + VD + LF / BEF / VIM followed by electroslag refining (ESR) if necessary for special purpose. Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers' requirements.
Bars are usually supplied bright in the annealed condition, or bright annealing specially.
Final heat treatment - Quenched and tempered. 
Stock Available: Round bar diam. 50 ~ 210mm, ESR ingot.
 
PRODUCT PROFILE & DIMENSIONS
Round bar & rod & disc (diameter): 5.5 ~ 950mm
Square bar & flat bar: 8 ~ 650mm
Plate & Sheet: cold & hot rolled / forged T 2.0 ~ 350 X W 10 ~ 1200 X L mm
 
MATERIAL SPECIFICATIONS - GJB 1951 - 94

TYPICAL CHEMICAL COMPOSITIONS (mass fraction - %)      
Carbon, C (%): 0.33 ~ 0.41
Manganese, Mn (%): 0.25 ~ 0.55
Silicon, Si (%): 0.17 ~ 0.37
Phosphorus, P (%) ≤: 0.025
Sulfur, S (%) ≤: 0.015
Chromium, Cr (%):  1.20 ~ 1.60
Nickel, Ni (%): 3.00 ~ 3.50
Vanadium, V (%): -
Molybdenum, Mo (%): -
Tungsten, W (%): -
Ferrum, Fe (%): balance.

MECHANICAL PROPERTIES - HOT WORKING, HEAT TREATMENT
Heat treatment temperature /℃| annealing: -.
Heat treatment temperature /℃| Normalizing:  -
Heat treatment temperature /℃| Quenching:  820 oil cooling
Heat treatment temperature /℃| Tempering : 525 ~ 575 oil or water cooling
Hardness after annealing, ≤ HBW:  179 ~ 269
Tensile strength, Rm ≥ MPa: 1080
Yield strength, Rp0.2 ≥ MPa: 930
Elongation, A5 ≥ (%): 10.0
Reduction of area, Z ≥ (%): 50.0
Impact strength, AKu ≥ J: 55
Hardness after final heat treatment / HBW:  320 ~ 388.
 
TECHNICAL SALES ASSISTANCE & SERVICE
20+ years Focus On Special Steel Manufacturing and processing.
Stock over 60 grades with a competitive price, along with cutting service for specific requirement.
Customizing special 
material is welcome.

We closely cooperate with the professional inspection partners to strictly control the quality and improve the quality manage system, and guarantee the goods delivery each time. It is proved that we are worth of trusting and will be the strategic partner of the supplying chains in the special steels field.

Hot search:

Previous page:15Ni2Cr1Mo15
Last page:最后一页

Share to: